We've been pushing much higher volumes at the plating shop lately and it's been very troublesome to find time to flash all of our silvered parts.
Anybody know any alternatives to flashing for protecting silvered parts?
Alternatives to flashing for silvered parts
Moderators: piaptk, tragwag, Steve E., Aussie0zborn
- FFrankensteinRecords
- Posts: 43
- Joined: Thu May 17, 2012 7:26 pm
- Location: United States
- Contact:
-
- Posts: 1852
- Joined: Sat Mar 11, 2006 8:23 am
- Location: Australia
- Contact:
Re: Alternatives to flashing for silvered parts
What kind of parts do you refer to?
- FFrankensteinRecords
- Posts: 43
- Joined: Thu May 17, 2012 7:26 pm
- Location: United States
- Contact:
Re: Alternatives to flashing for silvered parts
Fathers or masters
Co-worker doesn't like the idea of de-silvering all of them because he's worried that changing the molecular structure of the surface will affect quality if we ever need to make new mothers off of them.
Co-worker doesn't like the idea of de-silvering all of them because he's worried that changing the molecular structure of the surface will affect quality if we ever need to make new mothers off of them.